| Brand Name: | ECER Chemical |
| Model Number: | PDM-40PS |
| MOQ: | 1 Ton |
| Price: | Negotiable |
| Delivery Time: | 7-15 Days |
| Payment Terms: | T/T,L/C |
Paper mills struggle with sizing efficiency: AKD and ASA sizing agents fail to cure properly when anionic trash interferes, causing ink feathering, poor water resistance and customer complaints on packaging and writing grades.
Mills respond by adding more sizing agent, which is expensive and can cause slip and runnability problems on the machine.
CauseSizing agents are cationic emulsions that must adsorb onto fibers and orient correctly to form a hydrophobic barrier. Anionic trash competes for the same adsorption sites and destabilizes the sizing emulsion, forming sticky deposits instead of a sizing film.
The result is a double loss: sizing agent wasted on trash, and deposits that break the sheet at the press section.
SolutionThis PolyDADMAC pre-treats the furnish by neutralizing anionic trash before sizing addition, allowing AKD and ASA to adsorb on fibers efficiently. The result is higher sizing efficiency at lower addition rates.
In a fine paper mill, adding 200 g/ton of this polymer before AKD allowed the mill to cut AKD dose by 25% while improving Cobb value from 32 to 24 g/m², eliminating customer complaints about ink feathering.
Key Features| Parameter | Specification |
|---|---|
| Appearance | Colorless to light yellow liquid |
| Solid Content | 40% ± 1% |
| Viscosity (25℃) | 6000-10000 cps |
| Charge Density | 5.8-6.8 meq/g |
| pH (1% solution) | 4.0-6.0 |
| Density (25℃) | 1.05-1.09 g/cm³ |
| Recommended Dosage | 150-400 g/ton of paper |
| Typical Cobb Improvement | 20-30% lower |
For fine paper, packaging board and tissue machines using AKD or ASA sizing, especially those running recycled fiber with high DCS loads. Also effective in paper mill effluent clarification.
Selection GuideDose based on cationic demand before the sizing addition point. Start at 200 g/ton and adjust until sizing response is stable at minimum AKD/ASA use. If Cobb values still drift, check pH and alum levels before increasing polymer.
FAQQ1: Why is my AKD consumption so high? Anionic trash is consuming it. Neutralize the trash first with PolyDADMAC; most mills cut AKD use 20-30% within a week of correct dosing.
Q2: Where exactly should I add it? At the blend chest or machine chest, 3-5 minutes before the sizing agent addition point, giving the polymer time to scavenge trash.
Q3: Does it help with ASA hydrolysis issues? Indirectly yes. Less trash means less emulsion destabilization, so ASA hydrolyzes less before reaching the sheet.
Q4: Can it clarify paper mill effluent too? Yes, the same product works as a coagulant for white water and effluent treatment, simplifying your chemical inventory across the mill.